Induction Brazing Available to Purchase
-
Published:1993
Abstract
This article begins with a discussion on the principle of induction brazing and addresses applications, advantages, and limitations of the process. It provides information on the induction brazing equipment and solid-state induction generators that are used in induction brazing. The article illustrates several basic joint designs for induction brazing as well as typical coils and some frequent applications and lists joint parameters for parts which are to be brazed by induction heating. It concludes with a discussion on the effect of thermal expansion on stress in the joint.
J.F. Libsch, Induction Brazing, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 333–335, https://doi.org/10.31399/asm.hb.v06.a0001387
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.