Mechanical Properties of Soft-Interlayer Solid-State Welds[1] Available to Purchase
-
Published:1993
Abstract
Soft-interlayer solid-state welds that join stronger base metals have unique mechanical properties that are of fundamental interest and may be of critical importance to designers. This article discusses the mechanical properties of soft-interlayer solid-state welds and the implications of these behaviors to service stress states and environments. It describes the tensile loading of soft-Interlayer welds in terms of the effect of interlayer thickness on stress, interlayer strain, time-dependent failure, effect of base-metal properties, and effect of interlayer fabrication method. The article concludes with a discussion on multiaxial loading.
R.S. Rosen, M.E. Kassner, Mechanical Properties of Soft-Interlayer Solid-State Welds, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 165–172, https://doi.org/10.31399/asm.hb.v06.a0001352
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.