Abstract
Furnace brazing is a mass production process for joining the components of small assemblies with a metallurgical bond, using a nonferrous filler metal as the bonding material and a furnace as the heat source. This article presents the advantages and limitations of the furnace brazing and reviews three types of furnaces: continuous, semi-continuous, and batch. It presents three examples of the industrial applications of the furnace brazing: vacuum devices, jet engines, and automotive industries. The health and safety guidelines to be followed during the furnace brazing are also discussed.
Toshi Oyama, Howard Mizuhara, Furnace Brazing, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 330–332, https://doi.org/10.31399/asm.hb.v06.a0001386
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.