Skip Nav Destination
ASM Handbook
Welding, Brazing, and SolderingAvailable to Purchase
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter
Torch Brazing Available to Purchase
By
Charles E. Fuerstenau
Charles E. Fuerstenau
Lucas-Milhaupt, Inc.
Search for other works by this author on:
-
Published:1993
Page range:
328 - 329
Abstract
Torch brazing utilizes a fuel gas flame as a heat source for the brazing process. This article discusses the advantages, limitations, applications, and key techniques of torch brazing, and presents an overview of the equipment used.
You do not currently have access to this chapter.
Citation
Charles E. Fuerstenau, Torch Brazing, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 328–329, https://doi.org/10.31399/asm.hb.v06.a0001385
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Failure of a Brazed Joint in a Type 321 Stainless Steel Assembly Due to Inadequate Cleaning
ASM Failure Analysis Case Histories: Processing Errors and Defects
Brazing and Soldering of Cast Irons
Cast Iron Science and Technology
Brazing of Aluminum Alloys
Aluminum Science and Technology
Brazing
Metals Handbook Desk Edition (2nd Edition)
Brazing of Refractory and Reactive Metals
Welding, Brazing, and Soldering
Brazing of Stainless Steels
Welding, Brazing, and Soldering
Brazing of Aluminum Alloys
Welding, Brazing, and Soldering
Brazing of Conventional Titanium Alloys
Welding, Brazing, and Soldering