This article outlines the requirements and methods associated with the inspection of brazements. It emphasizes the incorporation of these requirements into the overall quality system. The article reviews the acceptance limits, design limitations, and nondestructive and destructive inspection techniques involved in the brazement inspection. Selected case studies are also provided for further reference.