Dissimilar Welds With Stainless Steels
-
Published:1993
Abstract
This article briefly describes the welding of various stainless steels to dissimilar steels. The stainless steels include austenitic stainless steels, ferritic stainless steels, and martensitic stainless steels. The dissimilar steels include carbon and low-alloy steels. In addition, the article provides information on the cladding of austenitic stainless steel to carbon or low-alloy steels.