Friction Surfacing Available to Purchase
-
Published:1993
Abstract
In the friction surfacing process, a rotating consumable is brought into contact with a moving substrate, which results in a deposited layer on the substrate. This article describes the process as well as the equipment used. It also provides information on the applications of the friction surface process.
E.D. Nicholas, Friction Surfacing, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 321–323, https://doi.org/10.31399/asm.hb.v06.a0001383