Energy Sources Used for Fusion Welding[1]
-
Published:1993
Abstract
Welding and joining processes are essential for the development of virtually every manufactured product. This article discusses the fundamentals of fusion welding processes, with an emphasis on the underlying scientific principles. It reviews the role of energy-source intensity and the width of the heat-affected zone in fusion welding processes. The article contains figures from which the properties of any heat source can be estimated readily.
Thomas W. Eagar, Energy Sources Used for Fusion Welding, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 3–6, https://doi.org/10.31399/asm.hb.v06.a0001332