Welding, Brazing, and Soldering
Abstract
This article focuses on the various criteria considered in the selection of product forms, joint types, solders, and filler metals for brazing and soldering of base material components.
Abstract
Cast irons and carbon steels are brazeable materials, although the brazeability of cast iron is lower than that of carbon steel. The article provides a detailed discussion on the brazeability of different types of cast iron (malleable iron, ductile iron, and gray iron), carbon steels, and dissimilar metals. It describes the factors considered in the selection of filler-metal for cast iron and carbon steel brazing, such as temperature and environment,...
Sign in
ASM members
Member Sign InAnatol Rabinkin, Practice Considerations for Brazing and Soldering, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.