Detailed analyses and test correlations are typically required to support design development, structural sizing, and certification. This article addresses issues concerning building block levels ranging from design-allowables coupons up through subcomponents, as these levels exhibit a wide variety of test-analysis correlation objectives. At these levels, enhanced analysis capability can be used most effectively in minimizing test complexity and cost while also reducing design weight and risk. The article discusses the examples of tests for which good correlative capability has shown significant benefit. These include notched (open and/or filled hole) tension and compression, inter/intralaminar shear and tension, and pin bearing....
Sign in
ASM members
Member Sign InAdam J. Sawicki, Testing and Analysis Correlation, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 344–352, https://doi.org/10.31399/asm.hb.v21.a0003391
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.