Adhesive bonding is used to assemble composite components into larger structures. Finished components that are damaged during assembly or service are often repaired with adhesive-bonding techniques. This article summarizes criteria for adhesive selection and illustrates typical secondary adhesively bonded joint configurations. It discusses the highly loaded joint considerations of adhesives. The article describes the epoxy adhesives commonly used for the bonding or repair of composite structures. It discusses the surface preparation of composites and metals, and honeycomb processing, including perimeter trimming, mechanical forming, heat forming, core splicing, contouring, and cleaning. The article presents basic steps involved in the adhesive-bonding...
Sign in
ASM members
Member Sign InFlake C. Campbell, Secondary Adhesive Bonding of Polymer-Matrix Composites, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 620–632, https://doi.org/10.31399/asm.hb.v21.a0003489
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.