Bonded Repair of Metal Structures Using Composites
-
Published:2001
Abstract
Composite bonded repair technology is based on the use of advanced composite repairs or reinforcements that are adhesively bonded to a damaged structure. This article discusses the key steps that are normally encountered in the design, certification, and application of an adhesively bonded repair. Some examples of successful repairs to military aircraft are also discussed.
Sign in
ASM members
Member Sign InRichard J. Chester, James J. Mazza, Bonded Repair of Metal Structures Using Composites, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 922–930, https://doi.org/10.31399/asm.hb.v21.a0003452