Abstract
Post-processing includes various processes that might be required to produce finished components from the ceramic-matrix composites (CMC) materials. The processes consist of machining or finishing operations, coating, joining, assembly operations, and nondestructive evaluation of CMCs and its components. This article discusses the specific needs for science and technology in these areas relative to the goal of employing CMCs in a variety of applications.
Sign in
ASM members
Member Sign InDavid Lewis, III, M. Singh, Post-Processing and Assembly of Ceramic-Matrix Composites, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 668–673, https://doi.org/10.31399/asm.hb.v21.a0003430
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.