Extrusion of Particle-Reinforced Aluminum Composites
By
William C. Harrigan, Jr.
William C. Harrigan, Jr.
MMC Engineering, Inc.
Search for other works by this author on:
-
Published:2001
Abstract
This article discusses the dies, such as shear-face dies, conical-feed dies, and bridge dies, that are used in extrusion of particle-reinforced aluminum composites. It provides an overview of the effects of reinforcements on the properties of aluminum composites.
You do not currently have access to this chapter.
Citation
William C. Harrigan, Jr., Extrusion of Particle-Reinforced Aluminum Composites, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 666–667, https://doi.org/10.31399/asm.hb.v21.a0003429
Download citation file:
Related Book Content
Metal-Matrix Composites
Lightweight Materials Understanding the Basics
Research and Development
Aluminum Extrusion Technology
Thermodynamics in Extrusion
Aluminum Extrusion Technology
Extrusion Press and Auxiliary Equipment
Aluminum Extrusion Technology
List of Formula Symbols
Extrusion (Second Edition)
Processing of Aluminum Metal-Matrix Composites
Aluminum Science and Technology
Primary Working
Titanium Physical Metallurgy, Processing, and Applications
Extrusion Die and Tooling
Aluminum Extrusion Technology
Process Control in the Aluminum Extrusion Plant
Aluminum Extrusion Technology
Statistical Process and Quality Control
Aluminum Extrusion Technology