Worldwide Repair Standardization Available to Purchase
-
Published:2001
Page range:
931 - 933
Abstract
This article describes the types of repair and presents reasons for avoiding damage to a structure or component during repair. It discusses the major standardization issues with emphasis on design, repair materials, repair techniques, and inspection.
You do not currently have access to this chapter.
Citation
K.B. Armstrong, Worldwide Repair Standardization, Composites, Vol 21, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 931–933, https://doi.org/10.31399/asm.hb.v21.a0003451
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Cold Spray Applications in Repair and Refurbishment for the Aerospace, Oil and Gas, and Power-Generation Industries
High Pressure Cold Spray Principles and Applications