A sandwich structure is comprised of layered composite materials formed by bonding two or more thin facings or facesheets to a relatively thick core material. This article describes the sandwich panel failure modes. It tabulates the nomenclature and definitions for loads, geometry, and material properties. The article illustrates critical strength-check locations for a flat sandwich panel. It discusses the analysis methods formulated for flat rectangular honeycomb panels; curved sandwich panel; and for each of the various sandwich panel failure modes. The article concludes with a discussion on flat panel stability analysis methods.
Sign in
ASM members
Member Sign InStephen Ward, Analysis of Sandwich Structures, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 308–320, https://doi.org/10.31399/asm.hb.v21.a0003388
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.