Automotive Applications of Metal-Matrix Composites Available to Purchase
By
Warren H. Hunt, Jr.
;
Warren H. Hunt, Jr.
Aluminum Consultants Group, Inc.
Search for other works by this author on:
Daniel B. Miracle
Daniel B. Miracle
Air Force Research Laboratory
Search for other works by this author on:
-
Published:2001
Page range:
1029 - 1032
Abstract
This article provides information on the applications of metal-matrix composites in engine components, brake system, and driveshaft. The components include pistons, cylinder liners, valves, pushrods, and connecting rods.
You do not currently have access to this chapter.
Citation
Warren H. Hunt, Jr., Daniel B. Miracle, Automotive Applications of Metal-Matrix Composites, Composites, Vol 21, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 1029–1032, https://doi.org/10.31399/asm.hb.v21.a0003484
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Failure of Wrist Pins in an Automotive Engine
Handbook of Case Histories in Failure Analysis
Broken Connecting Rod from a Motor Boat
ASM Failure Analysis Case Histories: Offshore, Shipbuilding, and Marine Equipment
Fatigue Fracture of a Fan Blade
Handbook of Case Histories in Failure Analysis
Fatigue Cracking of a 1040 Steel Crankshaft Because of Excessive Segregation of Nonmetallic Inclusions
ASM Failure Analysis Case Histories: Automobiles and Trucks
Metal-Matrix Composites: Atlas of Fractographs
Fractography
Metal-Matrix Composites
Lightweight Materials Understanding the Basics
Introduction to Composites
Composites
Introduction to Post-Processing and Assembly
Composites