Skip Nav Destination
ASM Handbook
Composites
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter
Failure Analysis of Ceramic-Matrix Composites
By
Michael G. Jenkins
University of Washington—Seattle
;
Michael G. Jenkins
Search for other works by this author on:
Raj N. Singh
University of Cincinnati
Raj N. Singh
Search for other works by this author on:
-
Published:2001
Abstract
Interpretation of failures of ceramic-matrix composites, and in particular continuous fiber reinforced ceramic-matrix composites is complicated by the complex structure of the composite material. This article describes the failure characteristics and evidence of failure mechanisms of these composites, with illustrations.
Topics
Composites,
Carbon-carbon composites,
Ceramic-matrix composites,
Composite laminates,
Metal-matrix composites,
Polymer-matrix composites,
Reinforcement structures,
Fiber-reinforced composites,
Continuous fiber-reinforced ceramic matrix composites,
Failure mechanisms and analysis,
Failure mode and effects analysis
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Michael G. Jenkins, Raj N. Singh, Failure Analysis of Ceramic-Matrix Composites, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 1000–1002, https://doi.org/10.31399/asm.hb.v21.a0003469
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Introduction to Failure Analysis
Composites
Applications of Ceramic-Matrix Composites
Composites
Thermal Analysis
Composites
Tensile Testing of Ceramics and Ceramic-Matrix Composites
Tensile Testing (Second Edition)
Case Histories
Composites
Introduction to Composites
Composites
Introduction to Post-Processing and Assembly
Composites