Abstract
This article focuses on the factors to be considered for selecting fasteners for joining carbon fiber composites. These considerations include corrosion compatibility, fastener materials, strength, stiffness, head configurations, importance of clamp-up, hole fit, and lightning protection.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Robert T. Parker, Mechanical Fastener Selection, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 651–658, https://doi.org/10.31399/asm.hb.v21.a0003427
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Castability and Product Design of Ductile Iron
Cast Iron Science and Technology
Mechanical Behavior
Elements of Metallurgy and Engineering Alloys
Adhesive Bonding and Mechanical Fasteners
Beryllium Chemistry and Processing
Machining and Assembly
Structural Composite Materials
Honeycomb-Cored Sandwich Structure Composites
Optical Microscopy of Fiber-Reinforced Composites
Tensile Testing of Metals and Alloys
Tensile Testing (Second Edition)
Fatigue Fracture
Understanding How Components Fail (Third Edition)
300-Series PM Stainless Steels
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Properties Needed for the Design of Static Structures
Materials Selection and Design
Engineering Plastics
Lightweight Materials Understanding the Basics