Mechanical Fastener Selection Available to Purchase
By
Robert T. Parker
Robert T. Parker
Boeing Commercial Airplane Company
Search for other works by this author on:
-
Published:2001
Page range:
651 - 658
Abstract
This article focuses on the factors to be considered for selecting fasteners for joining carbon fiber composites. These considerations include corrosion compatibility, fastener materials, strength, stiffness, head configurations, importance of clamp-up, hole fit, and lightning protection.
You do not currently have access to this chapter.
Citation
Robert T. Parker, Mechanical Fastener Selection, Composites, Vol 21, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 651–658, https://doi.org/10.31399/asm.hb.v21.a0003427
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Attributes of Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Castability and Product Design of Ductile Iron
Cast Iron Science and Technology
Mechanical Behavior
Elements of Metallurgy and Engineering Alloys
Machining and Assembly
Structural Composite Materials
Adhesive Bonding and Mechanical Fasteners
Beryllium Chemistry and Processing
Tensile Testing of Metals and Alloys
Tensile Testing (Second Edition)
Honeycomb-Cored Sandwich Structure Composites
Optical Microscopy of Fiber-Reinforced Composites
Engineering Plastics
Lightweight Materials Understanding the Basics
300-Series PM Stainless Steels
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Fatigue Fracture
Understanding How Components Fail (Third Edition)