Hole Drilling in Polymer-Matrix Composites Available to Purchase
-
Published:2001
Abstract
Good hole-drilling processes are key to joining composite parts with other composite parts or with metal parts. This article discusses the considerations for drilling polymer-matrix composites. It describes the use of power-feed drill motors and automated drilling/fastener installation equipment. The article provides a discussion on reaming, countersinking, and three recommended choices of cutting tools for producing a countersink in carbon/epoxy structure. The cutting tools include: standard carbide insert cutters, solid carbide cutters, or polycrystalline diamond (PCD) insert cutters. The article concludes with a discussion on inspection of hole quality.
Michael J. Paleen, Jeffrey J. Kilwin, Hole Drilling in Polymer-Matrix Composites, Composites, Vol 21, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 646–650, https://doi.org/10.31399/asm.hb.v21.a0003426
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.