This article discusses the historical background of composite construction in recreational equipment and sporting goods. It provides information on the applications of composites in baseball bats, tennis rackets, and golf clubs. The applications of composites in bicycling, winter sports, aquatic sports, track, field, and archery equipment are also discussed.