This article illustrates typical fractographic features for a number of different composite materials. It describes the differences in fracture characteristics due to different loading, material processing, and environmental conditions. The article presents fractographic data obtained from epoxy matrix materials. Minimal fractographic data from other brittle thermoset resin systems are also presented. The article discusses the interlaminar fracture of composites with ductile thermoplastic matrices. It also provides information on the translaminar fracture features of the composite materials.