Abstract
This article provides information on the classification of various composites manufacturing processes based on similar transport processes. The composites manufacturing processes can be grouped into three categories: short-fiber suspension methods, squeeze flow methods, and porous media methods. The article presents an overview of the modeling philosophy and approach that is useful in describing composite manufacturing processes.
Suresh G. Advani, E. Murat Sozer, Process Modeling, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 423–433, https://doi.org/10.31399/asm.hb.v21.a0003402