Polyester Resins
By
Tim Pepper
Tim Pepper
Ashland Chemical Company
Search for other works by this author on:
-
Published:2001
Page range:
90 - 96
Abstract
This article provides an overview of the various types of unsaturated polyester resins and low-profile additives. The resins include general-purpose resins, isophthalic resins, bisphenol A fumarate resins, chlorendic resins, and vinyl ester resin. The article describes the mechanical and electrical properties, thermal and oxidative stability, and chemical and ultraviolet (UV) resistance of polyester resins. It concludes with a discussion on the flame-retardant polyester resins.
You do not currently have access to this chapter.
Citation
Tim Pepper, Polyester Resins, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 90–96, https://doi.org/10.31399/asm.hb.v21.a0003363
Download citation file:
Related Book Content
Polyester and Vinyl Ester Coatings
Protective Organic Coatings
Porcelain Enameling of Aluminum Alloys
Aluminum Science and Technology
Introduction to Materials Characterization
Materials Characterization
Properties of Cast Aluminum Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Zinc-Rich Coatings
Protective Organic Coatings
Refractory Metals and Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Introduction to Engineering Plastics
Engineered Materials Handbook Desk Edition
Engineering Plastics—An Introduction
Characterization and Failure Analysis of Plastics
Low-Expansion Alloys
Metals Handbook Desk Edition (2nd Edition)
Properties of Cast Copper Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials