Constituent Materials Testing
-
Published:2001
Abstract
This article describes the most significant tests to characterize the properties of constituent materials. It discusses the chemical, physical, and mechanical tests for determining the properties of reinforcement fibers and fabrics. The article provides information on some of the basic materials used for thermoset and thermoplastic resin matrices. It reviews the identification of the individual characteristics of thermoset and thermoplastic resin along with the test methods normally used for their determination. The article contains a table that lists properties and tests for uncured and cured thermoset-matrix resins and prepregs.
Shari Bugaj, Constituent Materials Testing, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 749–758, https://doi.org/10.31399/asm.hb.v21.a0003441
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!