Book Chapter
Aircraft Applications Available to Purchase
By
Mark Wilhelm
Mark Wilhelm
Boeing Commercial Airplane Company
Search for other works by this author on:
-
Published:2001
Page range:
1057 - 1066
Abstract
This article provides information on the applications of fiber-reinforced composites in commercial and military aircrafts. It tabulates the composite components in various types of aircraft. The applications of the composites in the components of Boeing 727, 737, 757, 767, 777, and 777-200 are schematically illustrated.
You do not currently have access to this chapter.
Citation
Mark Wilhelm, Aircraft Applications, Composites, Vol 21, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 1057–1066, https://doi.org/10.31399/asm.hb.v21.a0003477
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Automated Tape Laying
Composites
Composites
Elementary Materials Science
Aerospace Applications—Example Fatigue Problems
Fatigue and Durability of Metals at High Temperatures
Tensile Testing of Fiber-Reinforced Composites
Tensile Testing (Second Edition)
Damage Tolerance
Composites
An Overview of Aircraft Accident Investigation and Component Failures
Analysis and Prevention of Component and Equipment Failures
Additive Manufacturing Applications in Aviation
Additive Manufacturing Design and Applications
Design with Composites
Materials Selection and Design
Maintainability Issues
Composites