Carbon Matrices
-
Published:2001
Abstract
This article describes the various pure forms of carbon matrices and the corresponding methods used to create them or incorporate them into a matrix of a composite. These forms include graphite, diamond, fullerenes, and nanotubes. The article discusses the three types of liquid precursors, namely, thermoplastic, thermosetting, and evaporative or solvent carriers. It provides a description of the advantages and limitations of various methods involved in chemical vapor infiltration. The article concludes with a discussion on matrix contribution to composite properties.
James Gary Pruett, Carbon Matrices, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 164–168, https://doi.org/10.31399/asm.hb.v21.a0003373