High-Temperature Applications
-
Published:2001
Abstract
High-temperature-resistant polymers are used in aerospace, electronic, and other applications that demand outstanding elevated-temperature physical and mechanical properties. This article discusses the general characteristics of condensation-type polyimides and polymerization of monomer reactants (PMR) polyimides. It provides information on the applications of PMR-15 with illustrations.
Sign in
ASM members
Member Sign InTito T. Serafini, Stephen C. Mitchell, High-Temperature Applications, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 1050–1056, https://doi.org/10.31399/asm.hb.v21.a0003476