Abstract
This article schematically illustrates a fiber placement system and provides information on the applications of fiber placement. It discusses materials and design considerations for fiber placement. The article provides information on techniques that can be used to eliminate areas of missing tows.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Don O. Evans, Fiber Placement, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 477–479, https://doi.org/10.31399/asm.hb.v21.a0003410
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Reinforcing Material Lay-Up Quality Control
Composites
Computer-Aided Design and Manufacturing
Composites