Abstract
This article schematically illustrates a fiber placement system and provides information on the applications of fiber placement. It discusses materials and design considerations for fiber placement. The article provides information on techniques that can be used to eliminate areas of missing tows.
You do not currently have access to this chapter.
Citation
Don O. Evans, Fiber Placement, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 477–479, https://doi.org/10.31399/asm.hb.v21.a0003410
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Reinforcing Material Lay-Up Quality Control
Composites
Computer-Aided Design and Manufacturing
Composites