Manual Prepreg Lay-Up Available to Purchase
-
Published:2001
Abstract
The prepreg hand lay-up process is a versatile, reliable, cost-effective, and high quality process for fabricating large or small components. This article discusses the technique characteristics and applications of the process. It describes the stages involved in the process of lay-up, namely, lay-up definition, ply-kit cutting, layup, debulking, and preparation for curing. The article concludes with a discussion on the component properties and design guidelines of the prepreg hand lay-up process.
Andrew Mills, Manual Prepreg Lay-Up, Composites, Vol 21, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 470–476, https://doi.org/10.31399/asm.hb.v21.a0003409