This article reviews the history of prepreg and ply cutting technologies and outlines the options available for creating the necessary data and for nesting, cutting, and kitting the plies. It discusses the ways in which these steps influence the workflow for various applications. The characteristics of prepreg and ply cutting methods are presented in a table.
You do not currently have access to this chapter.
Citation
Joe Lautner, Prepreg and Ply Cutting, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 466–469, https://doi.org/10.31399/asm.hb.v21.a0003408
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Engineering for Manufacturability and Integrity
Iron and Steel Castings Engineering Guide