Space Applications
-
Published:2001
Abstract
This article discusses composites for unmanned space vehicles and provides an overview of key design drivers, challenges, and environment for use of composites in spacecraft, launch vehicles, and missiles. It describes the design allowable properties of composite materials. The article provides information on the specific state-of-the-art applications of composite materials for spacecraft missiles and launch vehicles. A discussion on the key applications, including solid rocket motor casings, payload fairings, and payload support structures, is presented.
Suraj P. Rawal, John W. Goodman, Space Applications, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 1033–1042, https://doi.org/10.31399/asm.hb.v21.a0003475