Composites
Cyanate Ester Resins
-
Published:2001
Abstract
Cyanate ester resins are a family of high-temperature thermosetting resins that bridge the gap in thermal performance between engineering epoxy and high-temperature polyimides. This article discusses the chemistry, properties and characteristics of the cyanate ester resins. It describes the processing procedures for the cyanate ester resins and provides information on properties for selected applications, such as space applications, radomes, and printed circuit boards.
Sign in
ASM members
Member Sign InSusan Robitaille, Cyanate Ester Resins, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 126–131, https://doi.org/10.31399/asm.hb.v21.a0003367