Automotive Applications
-
Published:2001
Abstract
This article discusses the advantages of polymer matrix composite for automotive application in terms of design drivers, noise, vibration, harshness efficiency, process materials property constraints, safety and reliability, design optimization, structural and appearance requirements, recyclability, and processability. It describes the properties of high-volume composites used in automotive industries. The article provides a discussion on state-of-the-art and developing technologies in automotive field.
Nicholas J. Gianaris, Automotive Applications, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 1020–1028, https://doi.org/10.31399/asm.hb.v21.a0003474
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.