ASM Handbook
Composites
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter
Glass Fibers
By
Frederick T. Wallenberger
;
Frederick T. Wallenberger
PPG Industries, Inc.
Search for other works by this author on:
-
Published:2001
Publication history
December 01, 2001
Abstract
This article discusses the types, oxide composition, as well as mechanical and physical properties of general-purpose and special-purpose glass fibers. It describes the glass melting and fiber forming processes and provides information on important commercial products such as continuous roving, woven roving, fiberglass mat, chopped strand, and textile yarns.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Frederick T. Wallenberger, James C. Watson, Hong Li, Glass Fibers, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 27–34, https://doi.org/10.31399/asm.hb.v21.a0003353
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Glass Processing
Engineered Materials Handbook Desk Edition
Interfaces and Interphases
Composites
6042 Extrusion Alloy
Properties and Selection of Aluminum Alloys
3105 Sheet Alloy
Properties and Selection of Aluminum Alloys
5754 Al-3.1Mg Alloy
Properties and Selection of Aluminum Alloys
6351 Extrusion Alloy
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
1060 99.60 Aluminum Minimum
Properties and Selection of Aluminum Alloys