Abstract
This article focuses on the techniques used in recycling of aluminum metal matrix composites (MMCs) such as discontinuous SiC reinforced aluminum MMCs and continuous reinforced aluminum MMCs. It provides a discussion on the properties of recycled aluminum MMCs and disposal of aluminum MMCs.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
David Weiss, Recycling and Disposal of Metal-Matrix Composites, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 1013–1015, https://doi.org/10.31399/asm.hb.v21.a0003472
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Recycling
Elementary Materials Science
Extrusion of Hard Alloys
Aluminum Extrusion Technology
Recycling and Other Environmental Considerations for Ceramics and Glasses
Engineered Materials Handbook Desk Edition
Green Coatings
Protective Organic Coatings
Metal Matrix Composites
Structural Composite Materials
Hot Chamber Die Casting
Casting
Metal Cutting and Grinding Fluids
Machining