Book Chapter
Recycling and Disposal of Metal-Matrix Composites
By
-
Published:2001
Page range:
1013 - 1015
Abstract
This article focuses on the techniques used in recycling of aluminum metal matrix composites (MMCs) such as discontinuous SiC reinforced aluminum MMCs and continuous reinforced aluminum MMCs. It provides a discussion on the properties of recycled aluminum MMCs and disposal of aluminum MMCs.
You do not currently have access to this chapter.
Citation
David Weiss, Recycling and Disposal of Metal-Matrix Composites, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 1013–1015, https://doi.org/10.31399/asm.hb.v21.a0003472
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.
Related Book Content
Recycling
Elementary Materials Science
Aluminum Building Products
Aluminum: Technology, Industry, and Applications
Extrusion of Hard Alloys
Aluminum Extrusion Technology
Green Coatings
Protective Organic Coatings
Recycling and Other Environmental Considerations for Ceramics and Glasses
Engineered Materials Handbook Desk Edition
Mining, Refining, Smelting, and Recycling
Aluminum: Technology, Industry, and Applications
Metal Matrix Composites
Structural Composite Materials
Hot Chamber Die Casting
Casting