Book Chapter
Design Allowables
By
Chris Boshers
Chris Boshers
Composite Materials Characterization, Inc.
Search for other works by this author on:
-
Published:2001
Page range:
360 - 365
Abstract
This article discusses the need for design allowables, development of design allowables, and important factors that affect the selection of the allowable. It provides a comparison between lamina and laminate allowables. The article discusses laminate results and specific techniques used in the statistical development of allowable values.
You do not currently have access to this chapter.
Citation
Chris Boshers, Design Allowables, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 360–365, https://doi.org/10.31399/asm.hb.v21.a0003393
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Design Allowables for Static Metallic Material Properties
Mechanical Testing and Evaluation
Glossary of Filament-Winding Terms
Composite Filament Winding
Repair
Structural Composite Materials
Lamina and Laminate Mechanical Testing
Composites
Out-of-Plane Analysis
Composites
Custom Sailing Yacht Design and Manufacture
Composites
Overview of Testing and Certification
Composites
Fractography of Composites
Characterization and Failure Analysis of Plastics
Specifications and Designations of Fibers and Resins
Composite Filament Winding