Reinforcing Material Lay-Up Quality Control Available to Purchase
-
Published:2001
Abstract
In-process inspection during composite material lay-up is essential if the structural, dimensional, and environmental performance designed into a part is to be consistently achieved. This article discusses the requirements to be met by the facilities and equipment to produce high-quality composites. It reviews the procedures that are allowed and prohibited in controlled-contamination areas of lay-up. The article emphasizes significant areas, such as material control and lay-up process, in which quality-control personnel can be effective in preventing production problems. It concludes with a discussion on automated tape laying and fiber placement, as well as the numerically aided lay-up process.
Barry P. Van West, Reinforcing Material Lay-Up Quality Control, Composites, Vol 21, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 685–691, https://doi.org/10.31399/asm.hb.v21.a0003434
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.