Tooling and Assembly Quality Control
-
Published:2001
Abstract
Tooling and assembly methodologies for advanced composites have steadily improved as a result of advancements in materials, through the use of computer-aided design/computer-aided manufacturing technology, and through application of sophisticated design for manufacturing and assembly concepts. This article reviews techniques and technologies that are used to control the quality of tooling and assembly methods for composite components.
Sign in
ASM members
Member Sign InTooling and Assembly Quality Control, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 682–684, https://doi.org/10.31399/asm.hb.v21.a0003433