Skip Nav Destination
ASM Handbook Archive
CompositesAvailable to Purchase
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Volume 21 provides a working knowledge of the capabilities and applications of commercially significant composites, including metal-matrix composites, ceramic-matrix composites, and polymer and organic-matrix types. It covers constituent materials, design considerations, and manufacturing processes. It includes detailed information on post-processing and assembly, quality control, testing and certification, and properties and performance. In addition, the volume addresses product reliability and repair, failure analysis, and recycling and disposal. It provides application examples and engineering data as well. For information on the print version of Volume 21, ISBN 978-0-87170-703-1, follow this link.
Composites
Edited by: Daniel B. Miracle, Steven L. Donaldson
https://doi.org/10.31399/asm.hb.v21.9781627081955
ISBN (electronic): 978-1-62708-195-5
Publisher: ASM International
Published: 2001
Download citation file:
Table of Contents
-
Introduction to Composites
-
Introduction to CompositesByDaniel B. Miracle;Daniel B. MiracleAir Force Research LaboratorySearch for other works by this author on:Steven L. DonaldsonSteven L. DonaldsonAir Force Research LaboratorySearch for other works by this author on:Published:01 January 2001
-
-
Constituent Materials
-
Introduction to Constituent MaterialsBySteven R. NuttSteven R. NuttUniversity of Southern CaliforniaSearch for other works by this author on:Published:01 January 2001
-
Introduction to Reinforcing FibersByFrederick T. WallenbergerFrederick T. WallenbergerPPG Industries, Inc.Search for other works by this author on:Published:01 January 2001
-
Glass FibersByFrederick T. Wallenberger;Frederick T. WallenbergerPPG Industries, Inc.Search for other works by this author on:Published:01 January 2001
-
Aramid FibersByKarl K. ChangKarl K. ChangE.I. Du Pont de Nemours & Company, Inc.Search for other works by this author on:Published:01 January 2001
-
Ceramic FibersByH.M. YunH.M. YunNASA Glenn Research CenterSearch for other works by this author on:Published:01 January 2001
-
Discontinuous Reinforcements for Metal-Matrix CompositesByCory A. SmithCory A. SmithDWA Aluminum CompositesSearch for other works by this author on:Published:01 January 2001
-
Continuous Fiber Reinforcements for Metal-Matrix CompositesByColin McCulloughColin McCullough3M Company, Electrical Products DivisionSearch for other works by this author on:Published:01 January 2001
-
Epoxy ResinsByJohn D. NeunerJohn D. NeunerHexcel CorporationSearch for other works by this author on:Published:01 January 2001
-
Polyester ResinsByTim PepperTim PepperAshland Chemical CompanySearch for other works by this author on:Published:01 January 2001
-
Polyimide ResinsByDaniel A. ScolaDaniel A. ScolaUniversity of ConnecticutSearch for other works by this author on:Published:01 January 2001
-
Phenolic ResinsByShahid P. QureshiShahid P. QureshiGeorgia-Pacific Resins, Inc.Search for other works by this author on:Published:01 January 2001
-
Thermoplastic ResinsByLee McKagueLee McKagueComposites-Consulting, Inc.Search for other works by this author on:Published:01 January 2001
-
Carbon MatricesByJames Gary PruettJames Gary PruettHitco Carbon CompositesSearch for other works by this author on:Published:01 January 2001
-
Interfaces and InterphasesByLawrence T. DrzalLawrence T. DrzalMichigan State UniversitySearch for other works by this author on:Published:01 January 2001
-
Bio-Based Resins and Natural FibersByShrikant N. KhotShrikant N. KhotUniversity of DelawareSearch for other works by this author on:Published:01 January 2001
-
-
Engineering Mechanics, Analysis, and Design
-
Introduction to Engineering Mechanics, Analysis, and DesignByScott ReeveScott ReeveNational Composite CenterSearch for other works by this author on:Published:01 January 2001
-
Characterizing Strength from a Structural Design PerspectiveByS. ChristensenS. ChristensenThe Boeing CompanySearch for other works by this author on:Published:01 January 2001
-
Fracture Mechanics of Composite DelaminationByT. Kevin O'BrienT. Kevin O'BrienU.S. Army Research LaboratorySearch for other works by this author on:Published:01 January 2001
-
Hygrothermal BehaviorByDaniel R. RuffnerDaniel R. RuffnerThe Boeing CompanySearch for other works by this author on:Published:01 January 2001
-
Fatigue and Life PredictionByJeffrey R. SchaffJeffrey R. SchaffUnited Technologies Research CenterSearch for other works by this author on:Published:01 January 2001
-
Bolted and Bonded JointsByL.J. Hart-SmithL.J. Hart-SmithThe Boeing CompanySearch for other works by this author on:Published:01 January 2001
-
Instability ConsiderationsByGerald Flanagan;Gerald FlanaganMaterials Sciences CorporationSearch for other works by this author on:Carol MeyersCarol MeyersMaterials Sciences CorporationSearch for other works by this author on:Published:01 January 2001
-
Damage ToleranceByMike R. Woodward;Mike R. WoodwardLockheed Martin Aeronautics CompanySearch for other works by this author on:Rich StoverRich StoverLockheed Martin Aeronautics CompanySearch for other works by this author on:Published:01 January 2001
-
Out-of-Plane AnalysisByJonathan GoeringJonathan GoeringAlbany International Techniweave, Inc.Search for other works by this author on:Published:01 January 2001
-
Analysis of Sandwich StructuresByStephen WardStephen WardSW Composites; Lawrence Gintert, Concurrent Technologies CorporationSearch for other works by this author on:Published:01 January 2001
-
Finite Element AnalysisByNaveen RastogiNaveen RastogiVisteon Chassis SystemsSearch for other works by this author on:Published:01 January 2001
-
Computer ProgramsByBarry J. BerenbergBarry J. BerenbergCaldera CompositesSearch for other works by this author on:Published:01 January 2001
-
Testing and Analysis CorrelationByAdam J. SawickiAdam J. SawickiThe Boeing CompanySearch for other works by this author on:Published:01 January 2001
-
Design AllowablesByChris BoshersChris BoshersComposite Materials Characterization, Inc.Search for other works by this author on:Published:01 January 2001
-
Computer-Aided Design and ManufacturingPublished:01 January 2001
-
Design, Tooling, and Manufacturing InteractionByAnthony J. VizziniAnthony J. VizziniUniversity of MarylandSearch for other works by this author on:Published:01 January 2001
-
Cost AnalysisByStephen Mitchell;Stephen MitchellGeneral Electric Aircraft EnginesSearch for other works by this author on:Published:01 January 2001
-
Rapid PrototypingByDavid L. Bourell;David L. BourellThe University of Texas at AustinSearch for other works by this author on:Joseph J. Beaman, Jr.;Joseph J. Beaman, Jr.The University of Texas at AustinSearch for other works by this author on:Amit BandyopadhyayAmit BandyopadhyayWashington State UniversitySearch for other works by this author on:Published:01 January 2001
-
Design GuidelinesByLynda FioriniLynda FioriniXC Associates, Inc.Search for other works by this author on:Published:01 January 2001
-
Engineering Mechanics and Analysis of Metal-Matrix CompositesByBhaskar S. MajumdarBhaskar S. MajumdarNew Mexico Institute of Mining and TechnologySearch for other works by this author on:Published:01 January 2001
-
Fracture Analysis of Fiber-Reinforced Ceramic-Matrix CompositesByF.W. ZokF.W. ZokUniversity of California at Santa BarbaraSearch for other works by this author on:Published:01 January 2001
-
-
Manufacturing Processes
-
Introduction to Manufacturing of Polymer-Matrix CompositesByB. Tomas ÅströmB. Tomas ÅströmIFP SICOMP AB,SwedenSearch for other works by this author on:Published:01 January 2001
-
Process ModelingByE. Murat SozerE. Murat SozerKOC University,TurkeySearch for other works by this author on:Published:01 January 2001
-
Composite ToolingByLouis C. DorworthLouis C. DorworthAbaris Training Resources, Inc.Search for other works by this author on:Published:01 January 2001
-
Elastomeric ToolingByR.C. Adams;R.C. AdamsLockheed Martin Aeronautical SystemsSearch for other works by this author on:Marvin FostonMarvin FostonLockheed Martin Aeronautical SystemsSearch for other works by this author on:Published:01 January 2001
-
Open Molding: Hand Lay-Up and Spray-UpByFinn Roger AndresenFinn Roger AndresenReichhold AS,NorwaySearch for other works by this author on:Published:01 January 2001
-
Custom Sailing Yacht Design and ManufactureByRichard Downs-Honey;Richard Downs-HoneyHigh Modulus New Zealand LimitedSearch for other works by this author on:Mark BattleyMark BattleyIndustrial Research Limited,New ZealandSearch for other works by this author on:Published:01 January 2001
-
Prepreg and Ply CuttingByJoe LautnerJoe LautnerGerber Technology Inc.Search for other works by this author on:Published:01 January 2001
-
Manual Prepreg Lay-UpByAndrew MillsAndrew MillsComposites Manufacturing Research Centre, Cranfield University,United KingdomSearch for other works by this author on:Published:01 January 2001
-
Automated Tape LayingByMichael N. GrimshawMichael N. GrimshawCincinnati Machine, A UNOVA CompanySearch for other works by this author on:Published:01 January 2001
-
Resin Transfer Molding and Structural Reaction Injection MoldingByC.D. RuddC.D. RuddUniversity of NottinghamSearch for other works by this author on:Published:01 January 2001
-
Vacuum InfusionByArlen Hoebergen;Arlen HoebergenCentre of Lightweight Structures TUD-TNO,The NetherlandsSearch for other works by this author on:J. Anders HolmbergJ. Anders HolmbergSICOMP AB,SwedenSearch for other works by this author on:Published:01 January 2001
-
Compression MoldingByCharles W. Peterson;Charles W. PetersonAzdel bv,The NetherlandsSearch for other works by this author on:R. KühfuszR. KühfuszMenzolit-Fibron GmbH,GermanySearch for other works by this author on:Published:01 January 2001
-
Filament WindingPublished:01 January 2001
-
PultrusionByJoseph E. Sumerak;Joseph E. SumerakCreative Pultrusions Inc.Search for other works by this author on:Jeffrey D. MartinJeffrey D. MartinMartin Pultrusion GroupSearch for other works by this author on:Published:01 January 2001
-
Tube RollingByPaul A. RoyPaul A. RoyVantage Associates, Inc.Search for other works by this author on:Published:01 January 2001
-
Thermoplastic Composites ManufacturingByB. Tomas ÅströmB. Tomas ÅströmIFP SICOMP AB,SwedenSearch for other works by this author on:Published:01 January 2001
-
Processing of Ceramic-Matrix CompositesByK.K. Chawla;K.K. ChawlaUniversity of Alabama at BirminghamSearch for other works by this author on:N. ChawlaN. ChawlaArizona State UniversitySearch for other works by this author on:Published:01 January 2001
-
-
Post-Processing and Assembly
-
Introduction to Post-Processing and AssemblyByFlake C. CampbellFlake C. CampbellThe Boeing CompanySearch for other works by this author on:Published:01 January 2001
-
Machining, Trimming, and Routing of Polymer-Matrix CompositesByLawrence F. KuberskiLawrence F. KuberskiFischer U.S.A.Search for other works by this author on:Published:01 January 2001
-
Secondary Adhesive Bonding of Polymer-Matrix CompositesByFlake C. CampbellFlake C. CampbellThe Boeing Company—St. LouisSearch for other works by this author on:Published:01 January 2001
-
Processing and Joining of Thermoplastic CompositesByDouglas A. McCarville;Douglas A. McCarvilleBoeing Military Aircraft & Missile SystemsSearch for other works by this author on:Henry A. SchaeferHenry A. SchaeferBoeing Military Aircraft & Missile SystemsSearch for other works by this author on:Published:01 January 2001
-
Hole Drilling in Polymer-Matrix CompositesByMichael J. Paleen;Michael J. PaleenThe Boeing Company,St. LouisSearch for other works by this author on:Jeffrey J. KilwinJeffrey J. KilwinThe Boeing Company,St. LouisSearch for other works by this author on:Published:01 January 2001
-
Mechanical Fastener SelectionByRobert T. ParkerRobert T. ParkerBoeing Commercial Airplane CompanySearch for other works by this author on:Published:01 January 2001
-
Environmental Protection and SealingByLeslie A. HoeckelmanLeslie A. HoeckelmanThe Boeing Company,St. LouisSearch for other works by this author on:Published:01 January 2001
-
Extrusion of Particle-Reinforced Aluminum CompositesByWilliam C. Harrigan, Jr.William C. Harrigan, Jr.MMC Engineering, Inc.Search for other works by this author on:Published:01 January 2001
-
Post-Processing and Assembly of Ceramic-Matrix CompositesByDavid Lewis, III;David Lewis, IIINaval Research LaboratorySearch for other works by this author on:M. SinghM. SinghQSS Group, Inc., NASA Glenn Research CenterSearch for other works by this author on:Published:01 January 2001
-
-
Quality Assurance
-
Introduction to Quality AssuranceByGrover Aaron Henson, IIIGrover Aaron Henson, IIIDesign Alternatives Inc.Search for other works by this author on:Published:01 January 2001
-
Resin Properties AnalysisByJohn D. RussellJohn D. RussellAir Force Research LaboratorySearch for other works by this author on:Published:01 January 2001
-
Reinforcing Material Lay-Up Quality ControlByBarry P. Van WestBarry P. Van WestThe Boeing Company,SeattleSearch for other works by this author on:Published:01 January 2001
-
Cure Monitoring and ControlByPublished:01 January 2001
-
Nondestructive TestingByASM International Committee on Nondestructive Testing of CompositesASM International Committee on Nondestructive Testing of CompositesSearch for other works by this author on:Published:01 January 2001
-
Quality Assurance of Metal-Matrix CompositesByWilliam C. Harrigan, Jr.William C. Harrigan, Jr.MMC Engineering, Inc.Search for other works by this author on:Published:01 January 2001
-
-
Testing and Certification
-
Introduction to Testing and CertificationByRichard E. FieldsRichard E. FieldsLockheed Martin Missiles and Fire ControlSearch for other works by this author on:Published:01 January 2001
-
Overview of Testing and CertificationByRichard E. FieldsRichard E. FieldsLockheed Martin Missiles and Fire ControlSearch for other works by this author on:Published:01 January 2001
-
Constituent Materials TestingByShari BugajShari BugajFiberCote Industries, Inc.Search for other works by this author on:Published:01 January 2001
-
Lamina and Laminate Nonmechanical TestingByJohn MoylanJohn MoylanDelsen Testing LaboratoriesSearch for other works by this author on:Published:01 January 2001
-
Lamina and Laminate Mechanical TestingByRod WishartRod WishartIntegrated Technologies, Inc. (Intec)Search for other works by this author on:Published:01 January 2001
-
Element and Subcomponent TestingByLawrence A. GintertLawrence A. GintertConcurrent Technologies CorporationSearch for other works by this author on:Published:01 January 2001
-
Full-Scale Structural TestingByJohn E. McCartyJohn E. McCartyComposite Structures ConsultingSearch for other works by this author on:Published:01 January 2001
-
-
Properties and Performance
-
Properties and Performance of Polymer-Matrix CompositesPublished:01 January 2001
-
Properties of Metal-Matrix CompositesByDavid E. AlmanDavid E. AlmanU.S. Department of Energy, Albany Research CenterSearch for other works by this author on:Published:01 January 2001
-
Properties and Performance of Ceramic-Matrix and Carbon-Carbon CompositesByCynthia Powell DoğanCynthia Powell DoğanU.S. Department of Energy, Albany Research CenterSearch for other works by this author on:Published:01 January 2001
-
-
Product Reliability, Maintainability, and Repair
-
Introduction to Product Reliability, Maintainability, and RepairByRikard B. HeslehurstRikard B. HeslehurstAustralian Defence Force AcademySearch for other works by this author on:Published:01 January 2001
-
Designing for RepairabilityByR.B. HeslehurstR.B. HeslehurstAustralian Defence Force AcademySearch for other works by this author on:Published:01 January 2001
-
Repair Engineering and Design ConsiderationsByRikard B. Heslehurst;Rikard B. HeslehurstAustralian Defence Force AcademySearch for other works by this author on:Mark S. ForteMark S. ForteU.S. Air Force Research LaboratorySearch for other works by this author on:Published:01 January 2001
-
Repair Applications, Quality Control, and InspectionByMichael J. HokeMichael J. HokeAbaris Training Resources Inc.Search for other works by this author on:Published:01 January 2001
-
Ship Structure RepairsByA.J. RussellA.J. RussellDockyard Laboratory Pacific, DRDC,CanadaSearch for other works by this author on:Published:01 January 2001
-
Rehabilitation of Reinforced Concrete Structures Using Fiber-Reinforced Polymer CompositesByL. KahnL. KahnGeorgia Institute of TechnologySearch for other works by this author on:Published:01 January 2001
-
Maintainability IssuesByMark S. Forte;Mark S. ForteAir Force Research LaboratorySearch for other works by this author on:Rikard B. HeslehurstRikard B. HeslehurstAustralian Defence Force AcademySearch for other works by this author on:Published:01 January 2001
-
Bonded Repair of Metal Structures Using CompositesByRichard J. Chester;Richard J. ChesterAeronautical and Maritime Research Laboratory,AustraliaSearch for other works by this author on:James J. MazzaJames J. MazzaAir Force Research LaboratorySearch for other works by this author on:Published:01 January 2001
-
Worldwide Repair StandardizationPublished:01 January 2001
-
Product Reliability, In-Service Experience, and Lessons LearnedByPublished:01 January 2001
-
-
Failure Analysis
-
Introduction to Failure AnalysisByPatricia L. StumpffPatricia L. StumpffHartzell Propeller, Inc.Search for other works by this author on:Published:01 January 2001
-
Failure CausesByJohn E. MoalliJohn E. MoalliExponent Failure Analysis AssociatesSearch for other works by this author on:Published:01 January 2001
-
Failure Analysis ProceduresByPatricia L. StumpffPatricia L. StumpffHartzell Propeller, Inc.Search for other works by this author on:Published:01 January 2001
-
Visual Analysis, Nondestructive Testing, and Destructive TestingByPatricia L. StumpffPatricia L. StumpffHartzell Propeller, Inc.Search for other works by this author on:Published:01 January 2001
-
MicroscopyByLuther M. GammonLuther M. GammonThe Boeing CompanySearch for other works by this author on:Published:01 January 2001
-
FractographyByPatricia L. StumpffPatricia L. StumpffHartzell Propeller, Inc.Search for other works by this author on:Published:01 January 2001
-
Case HistoriesByPatricia L. StumpffPatricia L. StumpffHartzell Propeller Inc.Search for other works by this author on:Published:01 January 2001
-
Fatigue Properties and Quantitative Fractography of Metal-Matrix CompositesByBruce CrawfordBruce CrawfordDeakin University,AustraliaSearch for other works by this author on:Published:01 January 2001
-
Failure Analysis of Ceramic-Matrix CompositesByMichael G. Jenkins;Michael G. JenkinsUniversity of Washington—SeattleSearch for other works by this author on:Raj N. SinghRaj N. SinghUniversity of CincinnatiSearch for other works by this author on:Published:01 January 2001
-
-
Recycling and Disposal
-
Introduction to Recycling and Disposal of CompositesByNicholas J. GianarisNicholas J. GianarisVisteon CorporationSearch for other works by this author on:Published:01 January 2001
-
Recycling and Disposal of Polymer-Matrix CompositesByJohn M. HenshawJohn M. HenshawThe University of TulsaSearch for other works by this author on:Published:01 January 2001
-
Recycling and Disposal of Metal-Matrix CompositesByPublished:01 January 2001
-
-
Applications and Experience
-
Introduction to Applications for Advanced CompositesByTia Benson Tolle;Tia Benson TolleMaterials and Manufacturing Directorate, Air Force Research LaboratorySearch for other works by this author on:Warren H. Hunt, Jr.Warren H. Hunt, Jr.Aluminum Consultants Group, Inc.Search for other works by this author on:Published:01 January 2001
-
Automotive ApplicationsByNicholas J. GianarisNicholas J. GianarisVisteon CorporationSearch for other works by this author on:Published:01 January 2001
-
Automotive Applications of Metal-Matrix CompositesByWarren H. Hunt, Jr.;Warren H. Hunt, Jr.Aluminum Consultants Group, Inc.Search for other works by this author on:Daniel B. MiracleDaniel B. MiracleAir Force Research LaboratorySearch for other works by this author on:Published:01 January 2001
-
Space ApplicationsBySuraj P. Rawal;Suraj P. RawalLockheed Martin AstronauticsSearch for other works by this author on:John W. GoodmanJohn W. GoodmanMaterial Technologies, Inc.Search for other works by this author on:Published:01 January 2001
-
Aeronautical Applications of Metal-Matrix CompositesByDaniel B. MiracleDaniel B. MiracleAir Force Research LaboratorySearch for other works by this author on:Published:01 January 2001
-
High-Temperature ApplicationsByTito T. Serafini;Tito T. SerafiniGeneral Electric Aircraft EnginesSearch for other works by this author on:Stephen C. MitchellStephen C. MitchellGeneral Electric Aircraft EnginesSearch for other works by this author on:Published:01 January 2001
-
Aircraft ApplicationsByMark WilhelmMark WilhelmBoeing Commercial Airplane CompanySearch for other works by this author on:Published:01 January 2001
-
Applications of Carbon-Carbon CompositesByKristen M. KearnsKristen M. KearnsMaterials and Manufacturing Directorate, Air Force Research LaboratorySearch for other works by this author on:Published:01 January 2001
-
Thermal Management and Electronic Packaging ApplicationsByCarl ZwebenCarl ZwebenComposites ConsultantSearch for other works by this author on:Published:01 January 2001
-
Marine ApplicationsByC.P. GardinerC.P. GardinerDefence Science & Technology Organisation,AustraliaSearch for other works by this author on:Published:01 January 2001
-
Civil Infrastructure ApplicationsByVistasp M. KarbhariVistasp M. KarbhariUniversity of California,San DiegoSearch for other works by this author on:Published:01 January 2001
-
Applications of Ceramic-Matrix CompositesByPublished:01 January 2001
-
-
Supplementary Information