Effects of Composition, Processing, and Structure on Properties of Engineering Plastics
-
Published:1997
Abstract
This article discusses the most fundamental building-block level, atomic level, molecular considerations, intermolecular structures, and supermolecular issues. It contains a table that shows the structures and lists the properties of selected commodity and engineering plastics. The article describes the effects of structure on thermal and mechanical properties. It reviews the chemical, optical, and electrical properties of engineering plastics and commodity plastics. An explanation of important physical properties, many of which are unique to polymers, is also included. The factors that must be considered when processing engineering thermoplastics are discussed. These include melt viscosity and melt strength; crystallization; orientation, die swell, shrinkage, and molded-in stress; polymer degradation; and polymer blends.
A.-M.M. Baker, C.M.F. Barry, Effects of Composition, Processing, and Structure on Properties of Engineering Plastics, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 434–456, https://doi.org/10.31399/asm.hb.v20.a0002464
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.