This article provides a discussion on various types of glasses: traditional glasses, specialty glasses, and glass ceramics. It provides information on glazes and enamels and reviews the broad classes of ceramic materials. These include whitewares, structural clay products, technical ceramics, refractories, structural ceramics, engineering ceramics, and electronic and magnetic ceramics. General processing variables that can affect structure and compositional homogeneity are discussed. Traditional ceramics that include both oxide and nonoxide ceramics are also reviewed. The article concludes with several examples of engineering ceramics.
Sign in
ASM members
Member Sign InVictor A. Greenhut, Effects of Composition, Processing, and Structure on Properties of Ceramics and Glasses, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 416–433, https://doi.org/10.31399/asm.hb.v20.a0002463
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.