Materials Selection and Design
Design with Composites
-
Published:1997
Abstract
This article begins with a discussion on fiber-reinforced composite materials and describes the generic behavior and structure/property relationships of composites. The article summarizes lamina properties and presents equations that help in the calculation of lamina properties. Composite laminates are constructed from lamina with uniaxial fiber orientation and frequently from textile fabrics as well. The article explains the characteristics of symmetric in-plane and through-thickness laminates; asymmetric in-plane and symmetric through-thickness laminates; asymmetric laminates; and curved laminates. It provides information on controlled thermal expansion composites, metal-matrix composites, and ceramic-matrix composites. The article illustrates the types of bonded joints and concludes with...
Sign in
ASM members
Member Sign InR.J. Diefendorf, Design with Composites, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 648–665, https://doi.org/10.31399/asm.hb.v20.a0002478
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.