This article describes key processing methods and related design, manufacturing, and application considerations for plastic parts. The methods include injection molding, extrusion, thermoforming, blow molding, rotational molding, compression molding/transfer molding, composites processing, and casting. The article describes principal features incorporated into the design of plastic parts. It concludes with a discussion on the materials selection methodology for plastics.