Design for Ceramic Processing
-
Published:1997
Abstract
This article provides an overview of the steps that are used in ceramics processing and related mechanical design considerations. It discusses various design approaches, such as the empirical design, the deterministic design, and the probabilistic design. The article presents a general process design flowchart for ceramic processing. Information on traditional ceramics and advanced ceramics is also provided. The article describes various ceramic forming processes, such as wet processing, plastic forming, dry processing, and machining. The factors for evaluating different ceramic forming processes are summarized in a table. The article discusses vitrification and sintering that generally pertain to ceramic firing and concludes with a discussion on firing process factors.
Victor A. Greenhut, Design for Ceramic Processing, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 781–792, https://doi.org/10.31399/asm.hb.v20.a0002490
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.