Abstract
Manufacturing processes typically involve the reshaping of materials from one form to another under a set of processing conditions. This article discusses the two classification schemes of modeling for manufacturing processes, namely, on-line or off-line models and empirical, mechanistic, or deterministic models along with their important considerations. It describes the various aspects of modeling of deformation processes, casting operations, and fusion welding processes, with examples.
Sign in
ASM members
Member Sign InAnand J. Paul, Modeling of Manufacturing Processes, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 705–715, https://doi.org/10.31399/asm.hb.v20.a0002482
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.