Abstract
This article defines performance indices in a formal way and specifies how they are derived. The performance indices for a light, strong tie and a light, stiff beam are presented. The article presents two case studies that illustrate the use of material indices, shape factors, and selection charts to select materials.
Topics
Properties and performance
You do not currently have access to this chapter.
Citation
M.F. Ashby, Performance Indices, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 281–290, https://doi.org/10.31399/asm.hb.v20.a0002453
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Design Guidelines for Advanced High-Strength Steels
Advanced-High Strength Steels Science, Technology, and Applications
The Materials Selection Process
Metallurgy for the Non-Metallurgist (Second Edition)
Modeling of Diffusion Bonding
Metals Process Simulation
Materials for Advanced Steam Plants
Damage Mechanisms and Life Assessment of High-Temperature Components
Selection and Weldability of Non-Heat-Treatable Aluminum Alloys
Welding, Brazing, and Soldering
Erosion and Erosion-Corrosion
High-Temperature Corrosion and Materials Applications
Introduction to the Effects of Composition, Processing, and Structure on Materials Properties
Materials Selection and Design
Porous Powder Metallurgy Technology
Powder Metallurgy
Selection of Heat Treat Process for Optimum Gear Design
Heat Treatment of Gears A Practical Guide for Engineers
Selection of Materials for Tribosystems
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications